high-density polyethylene piping systems installer
Jump to:
High‑Density Polyethylene (HDPE) Piping Systems - Installer
High‑Density Polyethylene (HDPE) Piping Systems - Installer
The AWS High-Density Polyethylene (HDPE) Piping Systems Installer is designed to build validated, hands-on training and performance evaluations for professionals responsible for installing HDPE piping systems. It verifies fusion and assembly of skills.
The program includes structured technical training followed by a performance-based qualification assessment. Upon passing the exam, an AWS Performance-based Qualification Certificate (PQC) will be issued.
Professional Development Hours (PDHs) will be granted upon completion of the training. The HDPE Installer exam application and payment are separate from the training and are to be submitted to the designated AWS International Agent for scheduling of the assessment..
AT A GLANCE
32 Professional Development Hours Granted
(Day 5 is scheduled for the exam)
course details
-
Learning Objectives
-
Training Structure & Materials
-
Exam/Assessment
-
Registration & Pricing
The program is designed to:
- Qualify installers to perform HDPE jointing operations in accordance with approved procedures
- Provide essential understanding of HDPE materials, welding processes, and acceptance criteria
- Focus on hands-on skill development and workmanship quality
- Prepare candidates to successfully pass the Performance Qualification Test (PQT)
Participants completing the training should be able to:
- Perform butt fusion and electrofusion
- Prepare pipe ends and align joints
- Verify fusion parameters and bead quality
- Follow safety and installation procedures
- Meet project requirements for workmanship
In-Person, Private Group Training for Companies & Organizations
The HDPE Installer Training structure is hands-on, practical over four days, and on the fifth day, candidates take their test, followed by an evaluation and qualification decision.
In-Person, Individuals
The HDPE Installer Training structure is hands-on, practical over four days, and on the fifth day, the candidate takes their test, followed by an evaluation and qualification decision. Individual training offered in a group setting - upon request.
In the Middle East and North Africa region, in-person training with an exam will be Sunday–Thursday, 8:00 AM - 3:00 PM, and will be conducted in Al Khobar, Saudi Arabia (contact information: Bassam@eliteservies-int.com). For all other regions' training details, inquire at international@aws.org
Training Structure
Day 1 – Theoretical (essential knowledge only)
- HDPE material properties & classification
- Thermoplastic behavior (heating/cooling cycles)
- Jointing methods overview:
- Butt fusion & Electrofusion
- Approved procedure (step-by-step)
- Safety requirements (heating tools, pressure, environment)
- Acceptance criteria
Day 2–4 –Practical Training (hands-on) & Butt Fusion Qualification (primary).
Focused on Adhesive Bonded Joint Qualification
- Pipe preparation:
- Cutting
- Facing
- Alignment
- Heating plate usage:
- Temperature control
- Heating time
- Fusion process:
- Pressure application
- Bead formation control
- Cooling and removal
- Electrofusion basics (if included):
- Surface scraping
- Barcode input/control unit
- Repetition of joints under supervision
Day 5 – Performance Qualification Test (PQT)
- Practical test under controlled conditions
- Evaluation based on:
- Workmanship
- Joint quality
- Procedure compliance
- Feedback and qualification decision.
Materials
Participants will receive essential materials to support practical training and qualification:
- AWS–Elite HDPE Installation Procedure (Butt Fusion / Electrofusion – Qualified Methods)
- Simplified HDPE Fundamentals & Safety Guide
- Jointing Procedure Sheet (step-by-step execution)
- Welding Parameters Sheet (temperature, pressure, time)
- Acceptance Criteria & Visual Inspection Checklist
- Sample PQT Evaluation Form
- Practical Training Log Sheet
Training can focus on:
- Butt Fusion (as the primary method)
- Electrofusion (optional / upon request) Mechanical joints (overview only unless requested)
Professional Development Hours (PDHs)
Participants, upon completing training, will receive 32 PDHs.
Dates of Training
Current in-person training is scheduled at Elite Engineering in Saudi Arabia: November 1 -5, 2026 - with the assessment date to follow.
To register for an upcoming training in the Middle East and North Africa region, contact Bassam Abd Al Azeem, Elite Engineering, AWS International Agent at bassam@eliteservies-int.com.
For training outside of the Middle East and North Africa region, send an inquiry to international@aws.org to be connected with an eligible AWS International Agent.
Performance Qualification Test (PQT)
Upon completion of HDPE Installer training, candidates shall undergo a Performance Qualification Test (PQT) to evaluate their ability in:
- Fusion machine setup
- Butt fusion
- Electrofusion
- Workmanship and safety compliance
Exam Application
Submit your exam application and payment to the AWS International Agent portal that conducted your training.
Credentialing Issued
Upon a successful passing score on the assessment, the candidate shall be issued an AWS HDPE Installer Performance-based Qualification Certificate (PQC), which will define:
- Qualified jointing method
- Pipe size range
- Material classification
- Qualification date
Current exam date scheduled at Elite Engineering in Saudi Arabia: November 14, 2026
NOTICE: American Welding Society Certificate Authentication
If you successfully pass the examination, the American Welding Society (AWS) will issue an official certificate recognizing the credential*. Each certificate bears the official AWS logo, seal, authorized signature, and credential earned and is issued directly by AWS Headquarters, confirming its authenticity and industry recognition.
No AWS agent, independent contractor/representative, or third party is authorized to CREATE OR REPRODUCE credentials* on behalf of the American Welding Society. If you, as a candidate, receive something other than an official AWS issued credential*, please notify us at international@aws.org.
* Includes physical or digital copies of an AWS certification certificate, card or stamp, and assessment-based (ABC) or performance-based qualification (PQC) certificates.
Training Pricing
In-person private group training, for companies and organizations, and individual training (in a group setting) - pricing is upon request.
For training inquiries or to get registered for an upcoming training in the Middle East and North Africa region, contact Bassam Abd Al Azeem, Elite Engineering, AWS International Agent at bassam@eliteservies-int.com.
For training outside of the Middle East and North Africa region, send an inquiry to international@aws.org to be connected with an eligible AWS International Agent.
Exam/Assessment Price
Pricing for the HDPE Installer Assessment in the Middle East and North Africa region is $870 + 15% VAT.
For regions not mentioned above, please seek pricing directly from the designated AWS International Agent.
To register for the exam, submit your application and payment to the AWS International Agent portal that conducted your training.
For additional information, contact AWS International at international@aws.org
Frequently Asked Questions
-
What is an AWS International custom-designed and private, group training?
The AWS Custom Training Program is a tailored training solution designed to meet the specific skill development and certification needs of an organization, rather than using a standard, one-size-fits-all curriculum.
It allows companies and organizations to work directly with Subject Matter Experts (SME) to modify course content, delivery methods (such as on-site or virtual), and learning objectives to address unique operational challenges, or industry standards, ultimately enhancing workforce competency and compliance.
-
How can my company or organization schedule a private group training OR an AWS custom-designed training?
Simply send a request to our international team at international@aws.org detailing what training program you are interested in (for a private, group training program that is listed on our site) OR share your needs for an AWS custom-designed training program to meet your needs.
-
What is the difference between an AWS Certification and an Assessment-based Certificate?
AWS Certification programs focus on assessments conducted by its program that are independent of a specific class, course, education/training program, and of any provider of classes, courses, or programs. Whereas, Assessment-based Certificate Programs focus on education/training with assessment(s) used to confirm participants have achieved the intended learning outcomes.
The assessments associated with certifications are not designed to evaluate accomplishments of the intended learning outcomes of a specific class, course, or other education/training program or event, and the certifier is not the sole provider of any education or training that may be required for its certification. Where the Assessment-based Certificate program is based on specific training and its learning outcomes.
-
What is the difference between an AWS Assessment-based exam and a Performance-based Qualification exam?
An AWS Assessment-based is an exam evaluating your knowledge based on the training just received. An AWS Performance-based Qualification is an exam evaluating your ability to demonstrate the skillset. It’s performance based vs knowledge based.
-
How do individuals get registered for a private group and/or custom designed training?
Currently private group and custom-designed training programs are exclusive to companies, organizations and government agencies.
If you work for a company that would benefit from our international training programs, suggest that they reach out to our international team to explore the opportunities.