B2 Committee on Procedure & Performance Qualification

B2 Committee on Procedure & Performance Qualification

SCOPE

Responsible for creating and revising standards on procedure and performance qualification.

Committee Leadership

Chair

Tracy Davenport, PPCP, Inc.

Coordinator

VIvian Perez

Join the committee

Join the committee

The B2 Committee seeks volunteers to participate in its standards development process. The committee is recruiting all types of members as well as members with specific interests (Educators and General Interest) in regard to the committee’s scope. Contact Jennifer "Jen" Padron to learn more about this committee’s work and/or complete the Technical Committee Application.

As part of the standards development process, joining this committee will give you access to Accuris Engineering Workbench to streamline your workflow.

PUBLISHED DOCUMENTS

AWS B2.1/B2.1M:2026

Specification for Welding Procedure and Performance Qualification

This specification provides the requirements for qualification of welding procedure specifications, welders, and welding operators for manual, semiautomatic, mechanized, and automatic welding. The welding processes included are electrogas welding, electron beam welding, electroslag welding, flux cored arc welding, gas metal arc welding, gas tungsten arc welding, laser beam welding, oxyfuel gas welding, plasma arc welding, shielded metal arc welding, stud arc welding, and submerged arc welding. Base metals, filler metals, qualification variables, welding designs, and testing requirements are also included.

AWS B2.2/B2.2M:2026

Specification for Brazing Procedure and Performance Qualification

This specification provides the requirements for qualification of brazing procedure specifications, brazers, and brazing operators for manual, mechanized, and automatic brazing. The brazing processes included are torch brazing, furnace brazing, diffusion brazing, resistance brazing, dip brazing, infrared brazing, and induction brazing. Base metals, brazing, filler metals, brazing fluxes, brazing atmospheres, and brazing joint clearances are also included.

AWS B2.3/B2.3M:2026

Specification for Soldering Procedure and Performance Qualification

This specification provides the requirements for qualification of soldering procedure specifications, solderers, and soldering operators for manual, mechanized, and automatic soldering. The soldering processes included are torch soldering, furnace soldering, induction soldering, resistance soldering, dip soldering, iron soldering, and infrared soldering. Base metals, soldering filler metals, soldering fluxes, soldering atmospheres, and soldering joint clearances are also included.

AWS B2.4:2023

Specification for Welding Procedure and Performance Qualification for Thermoplastics

This specification provides the requirements for qualification of welding procedure specifications and welders for manual, semiautomatic, mechanized, and automatic welding. The welding processes included are electrofusion, hot gas, socket fusion, butt contact fusion, infrared, extrusion welding, flow fusion welding, and solvent cement welding. Base materials, filler materials, qualification variables, and testing requirements are also included.

B2.1-XX-XXX Series

85+ Standard Welding Procedure Specifications

AWS B2.5/B2.5M:2021

Specification for Measurement of Welding Power Source Output for Calculation of Welding Procedure Heat Input

This document provides methods for determination of welding heat input, both in the case of traditional welding systems and those employing waveform-controlled welding. It is intended that this specification be referenced by other qualification and fabrication welding standards requiring the measurement and calculation of heat input for maintenance of distortion and weldment properties such as strength, toughness, and corrosion-resistance.

List of Subcommittees

AWS B2A Subcommittee on Brazing Qualification

Chair: Terry Mueller, Motion Engineering, Ltd.

AWS B2B Subcommittee on Welding Qualification

Chair: Tracy Davenport, PRL Industries, LLC

AWS B2C Subcommittee Materials

Chair: Mike Bermasek, C-SPEC

AWS B2D Subcommittee on Standard Welding Procedure Specifications

Chair: Jim Sekely, Consultant

AWS B2E Subcommittee on Soldering Qualification

Chair: Terry Mueller, Motion Engineering, Ltd.

AWS B2F Subcommittee on Plastic Welding Qualification

Chair: Leah Dockter, Wegener Welding, LLC

AWS B2G Subcommittee on Procedure Qualification Records

Chair: Jim Sekely, Consultant

AWS B2H Subcommittee on Arc Energy

Chair: Terry Mueller, Motion Engineering, Ltd.