The G1 Committee seeks volunteers to participate in its standards development process. The committee is recruiting all types of members as well as members with specific interests (Consultants and General Interest) in regard to the committee’s scope. Contact Steve Hedrick to learn more about this committee’s work and/or complete the Technical Committee Application.
PUBLISHED DOCUMENTS
AWS G1.2M/G1.2:1999
Specification for Standardized Ultrasonic Welding Test Specimen for Thermoplastics
AWS G1.6:2022
Specification for the Training, Qualification, and Company Certification of Thermoplastic Welding Inspector Specialists and Thermoplastic Welding Inspector Assistants
AWS G1.10M:2016
Specification for the Qualification of Plastics Welding Inspectors for Hot Gas, Hot Gas Extrusion, and Heated Tool Butt Thermoplastic Welds (Historical)
HISTORICAL DOCUMENTS