∗ Welcome to the January  Issue of the Welding Journal. Please use your Member Number and Password and Log in to access this issue or   Welding Journal articles from past months. To secure an AWS Member Number, Join AWS Today! If you already are a member, please first Log in using your AWS member number.
AWS Welding Research papers (*) are available without Member login.


WJ Cover January 2007
January 2007

FEATURES

Investing in Welding's Future
Individuals, industry, and the Society move forward to build a solid foundation for the future of welding
Welding Superalloys for Aerospace Applications
Basic guidelines are provided for the successful welding of superalloys critical to aircraft and aerospace components
D. J. Tillack

Electron Beam Brazing for In-Space Construction
Researchers at Goddard Space Flight Center are working on an electron beam brazing process that can be used for in-space construction
Y. Flom

What's New in Cutting
The latest developments in cutting products are highlighted
A. Cullison et al.

Laser Engineered Net Shaping Advances Additive Manufacturing and Repair
The Lens Engineered Net Shaping process is becoming accepted for a variety of repairs and freeform fabrications
R. P. Mudge and N. R. Wald

WELDING RESEARCH SUPPLEMENT


A New Proposal of HAZ Toughness Evaluation Method - Part 1:HAZ Toughness of Structural Steel in Multilayer and Sinle-Layer Weld Joints (.pdf)
A method using single-layer welds proved useful for estimating HAZ toughness of construction structural steels
H. Furuya et al.

Measuring On-Line and Off-Line Noncontact Ultrasound Time of Flight Weld Penetration Depth (.pdf)
A variety of time of flight techniques were evaluated for measuring weld penetration depth
A Kita et al.

Effects of Fusion Zone Size and Failure Mode on Peak Load and Energy Absorbtion of Advanced High-Strength Steel Spot Welds (.pdf)
Two advanced high-strength steels were studied to determine the critical fusion zone size for nugget pullout
X. Sun et al.

Tailoring Fillet Weld Geometry Using a Genetic Algorithim and a Neural Network Trained with Convective Heat Flow Calculations (.pdf)
A real-number-based genetic algorithm and a neural network can be used to quickly determine the welding variable combinations needed to achieve a target gas metal arc fillet weld geometry
A. Kurmar et al.



Departments

Press Time News

Editorial

News of the Industry

International Update

Technology

Stainless Q&A

New Products

Brazing Q&A

Conferences

Coming Events

Welding Workbook

Society News

Tech Topics

Guide to AWS Services

Personnel

New Literature

Classifieds

Advertiser Index

Welding Journal (ISSN 0043-2296) is published monthly by the American Welding Society for $120.00 per year in the United States and possessions, $160 per year in foreign countries: $7.50 per single issue for AWS members and $10.00 per single issue for nonmembers. American Welding Society is located at 550 NW LeJeune Rd., Miami, FL 33126-5671; telephone (305) 443-9353. Periodicals postage paid in Miami, Fla., and additional mailing offices. POSTMASTER: Send address changes to Welding Journal, 550 NW LeJeune Rd., Miami, FL 33126-5671.

Readers of Welding Journal may make copies of articles for personal, archival, educational or research purposes, and which are not for sale or resale. Permission is granted to quote from articles, provided customary acknowledgment of authors and sources is made.

Copyright © 2007 by American Welding Society in both printed and electronic formats. The Society is not responsible for any statement made or opinion expressed herein. Data and information developed by the authors of specific articles are for informational purposes only and are not intended for use without independent, substantiating investigation on the part of potential users.

For permission to use Copyright information please contact Copyright.com