Mechanical Modeling of
Ultrasonic Welding
Analytical and numerical modeling of spot ultrasonic welding on thin
metal foils is motivated by a new ultrasonic rapid prototyping
technology
BY C. DOUMANIDIS AND Y. GAO
Posted 3/04 | Published 04/04
Liquation Cracking in
Full-Penetration Al-Mg-Si Welds
A higher fraction solid in the weld metal than in the partially melted
zone during terminal solidification is a necessary condition for
cracking to occur
BY C. HUANG AND S. KOU
Posted 3/04 | Published 04/04
Development and
Evaluation of an
In-Situ Beam Measurement for Spot Welding Lasers
Comparative measurements demonstrate that multiple shots on Kapton™
film yield a focused laser beam diameter that is 99% of the actual beam
diameter
BY P. W. FUERSCHBACH, J. T. NORRIS, R. C. DYKHUIZEN, AND A. R. MAHONEY
Posted 4/04 | Published 05/04
Three-Dimensional Simulation
of Transient
GMA Weld Pool with Free Surface
A 3-D transient thermo-fluid model with free surface can analyze
droplet flow effects on weld pool formation and weld bead profile
such as finger-like penetration and weld toe radius
BY Z. CAO, Z. YANG, AND X. L. CHEN
Posted 5/04 | Published 06/04
Reliability of Weld
Microstructure and Property Calculations
The 2004 AWS Adams Lecture explored whether experimentation is required
when developing consumables for new steels, or if modeling is
sufficient
H. K. D. H. BHADESHIA
Posted 8/04 | Published 9/04
Signature Analysis for Quality
Monitoring in
Short-Circuit GMAW
An effective method has been developed to identify the process
stability and weld quality of short-circuit GMAW
BY Y. X. CHU, S. J. HU, W. K. HOU, P. C. WANG AND S. P. MARIN
Posted 11/04 | Published 12/04
Intelligent Control of
Pulsed GTAW with Filler Metal
A visual imaging system provides feedback on weld shape for controlling
welding on plates with varied root openings
BY G. J. ZHANG ET AL.
Posted 12/04 | Published 1/05
Liquation Cracking in Full
Penetration Al-Si Welds
An investigation showed high-Si, Al-Si casting alloys could backfill
and heal liquation cracks in welds no matter which filler metal was
used
BYG. CAO AND S. KOU