2007 Expo - IBSS Page
|
This Symposium will make
available its latest technical abstracts
received and will be presented by experts in the field of Brazing and
Soldering.
Register online check code #W87 - Remember this is a free event. TUESDAY,
NOVEMBER 13,
2007 - 8:30 AM - 12:10 PM
8:30 AM CASE STUDY: FAILURE ANALYSIS OF SOLDER JOINTS ON A CONNECTOR ASSEMBLY Dr. Paul T. Vianco, Sandia National Laboratories, Albuquerque, NM 8:50 AM DEVELOPMENT AND CHARACTERIZATION OF AMORPHOUS FILLER METALS FOR JOINING OF MAGNESIUM ALLOYS Dr. Silke Muecklich, Institute of Composite Materials and Surface Technology, University of Technology, Chemnitz, Germany 9:10 AM SOLDERABILITY TESTING OF PB-FREE SOLDER ALLOYS VERSUS SN63-37PB EUTECTIC SOLDER FOR HIGH RELIABILITY APPLICATIONS Eddie P. Lopez,, Sandia National Laboratories, Albuquerque, NM 9:30 AM ADVANCES IN BRAZING AND SOLDERING WITH REACTIVE MULTILAYER FOIL APPLICATIONS Timothy P. Weihs, Reactive NanoTechnologies, Inc., Hunt Valley, MD 9:50 AM JOINING OF HIGH STRENGTH ALUMINUM BASED LIGHTWEIGHT MATERIALS WITH TIN BASED MMC SOLDERS Dip.-Ing. Sebastian Weis, Institute of Composite Materials and Surface Technology, University of Technology, Chemnitz, Germany 10:10 AM ULTRASONIC SOLDERING AND BRAZING Tim Frech, Edison Welding Institute, Columbus, OH 10:30 AM THE ARC SPRAY APPLICATION OF BRAZE MATERIAL TO COPPER/BRASS HEAT EXCHANGER COMPONENTS Peter T. Kutsopias, Praxair and TAFA, Grapevine, TX 10:50 AM ULTRASONIC IMAGING AND QUANTITATIVE ANALYSIS OF DEFECTS IN AG-CU-ZR ACTIVE BRAZE JOINTS Dr. Donald F. Susan, Sandia National Laboratories, Albuquerque, NM 11:10 AM FUNDAMENTAL STUDIES FOR JOINING YTTRIA STABILIZED ZIRCONIA (YSZ) TO CROFER22-APU BY REACTIVE BRAZING Oscar A. Quintana, University of Illinois at Chicago, Chicago, IL 11:30 AM CORROSION TESTING OF BNI-3 BRAZED SURFACES ON TYPE 347 STAINLESS STEEL FOR THE SPACE STATION INTERNAL COOLING SYSTEM Matt J. Pohlman and C. S. Jeffcoate, Honeywell Aerospace, Torrance, CA 11:50 AM SAFETY IN CUTTING, BRAZING & WELDING WITH ACETYLENE & OXYGEN Dr. Jesse A. Grantham, Welding & Joining Management Group, Westminster, CO TUESDAY, NOVEMBER 13, 2007 - 1:00 PM - 3:40 PM BRAZING & FORMING TECHNOLOGY PRODUCE ECONOMICAL HIGH TEMPERATURE OVEN TRAYS William J. Powers, HiTech Meta, Inc., Cleveland, OH 1:20 PM FLUORIDE ION CLEANING AS A PRE-BRAZE PROCESS Robert E. Kornfeld, High-Tech Furnace System, Inc., Shelby Township, MI 1:40 PM INNOVATIONS FOR THE MANUFACTURE OF INDUSTRIAL HEAT EXCHANGERS Dientje Fortuna, Sulzer Metco (US) Inc., Troy, MI 2:00 PM VIRTUAL REALITY TRAINER: HELPING TO CERTIFY FASTER AND BETTER Claude Choquet, 123certification, Inc., Montreal, Quebec, Canada 2:20 PM ADVANTAGES OF FLUX CORED ALLOYS IN OPEN AIR BRAZING Creed F. Darling, Lucas-Milhaupt, Inc., Cudahy, WI 2:40 PM AN INVESTIGATION OF POROSITY IN THE BRAZING OF COPPER USING NICUMAN 37: ROOT-CAUSE AND REMEDY Edgar G. Vanegas Hurtado, WESGO Metals, Hayward, CA 3:00 PM COMPARISON OF METAL-CERAMIC BRAZING METHODS Charles A. Walker, Sandia National Laboratories, Albuquerque, NM 3:20 PM HIGH STRENGTH, DUCTILE BRAZE REPAIRS FOR STATIONARY GAS TURBINE COMPONENTS Warren Miglietti, University of Pretoria and GE Aviation and M. Du Toit, University of Pretoria 3:40 PM STUDY ON THE WETTING OF GLASS-TO-METAL JOINING Prof. Cheng-Hsien Kuo, National Chiao Tung University, Hsinchu, Taiwan |



Our Sponsor
