TITLE OF POST   : WELDER/ FABRICATOR ( Skilled Workman)
NAME    : PATEL DARPAN VITHTHAL BHAI
PERMANENT ADDRESS  : At & Po: Menpura

        Ta : Dabhoi.
        Dist : Baroda-391 220.
        Gujarat , India.

E-MAIL ADDRESS   : darpan11@yahoo.com
PHONE NUMBER   : ( 091) ( 2663 ) 71701 (Residence)
NATIONALITY   : Indian
MARTIAL STATUS   : Unmarried
DATE OF BIRTH   : 22 DEC,1974.
PASSPORT NUMBER  : T-303072
LANGUAGE KNOWN  : English, Hindi, & Gujarati.
QUALIFICATION   : (1) Passed S.S.C. In March 1990 With 58% Marks.

        (2) Passed H.S.C In March 1992 With 53% Marks.

        (3) Down hill welding by M.A.W. course done inA.V.T.S.

        (Industrial Training Institute)

        (4) Aluminium T.I.G. welding course done in A.V.T.S.

        (Industrial Training Institute)

          EXPERIENCE  : Working With Larsen & Toubro Ltd. Baroda Since 2nd April 1993. Basic Training Period - 3 Years (April 1993 To March 1996).The Training Programme Was Designed To Develop Multi-Skills & Included Extensive 'Hands-On' Exercise. Training Was Imparted In All Areas In The Workshop - Fabrication, Welding , Griding , Polishing , Machining…..At Present Working With Larsen & Toubro Ltd as a "Multi Skilled Technician" With Effect From April' 02, 1996.

          TECHNICAL SKILL  : I Am Trained As A Qualify Multi Skilled Technician For Welder / Grinder / Fabricator And Interpret Drawing. I can do Marking, Different Way Of Cutting, GasCutting, Plasma Cutting And Good Setup.  

My Specialization Is In Welding . My Welding Qualification Data Is BELOW.                                 QUALIFICATION DATA 

          PROCESS CURRENT POLARITY POSITION QUAL. IN BASE MATERIAL THK. OF WLD. MAT. WITNESSED BY
          SMAW DCEP 3GUP P1 TO P11 28MM L&T
          GTAW DCEN 3GUP P1 TO P11 10MM L&T
          GTAW DCEN 2G P1 TO P11 12MM L&T
          GTAW DCEN 1G P1 TO P11 12MM LRIS
          GTAW DCEN 3GUP P1 TO P11 12MM LRIS
          GTAW + SMAW DCEN + DCEP 1G P1 TO P11 GTAW-5.2 MM SMAW-14.8 MM PDIL
          GTAW AC 1G P21 TO P25 36MM L&T
          GTAW DCEN 6G P1 TO P11 7.82MM L&T
          GTAW AC 6G P21 TO P25 14.2 MM L&T
          GTAW AC 1GR P21 TO P25 8.0 MM L&T
          GTAW AC 3GUP P21 TO P25 36 MM UDHE

    * ALUMINIUM WELDING EXPERIENCE FOR DEFENCE JOB ( Helicopter Fuel Tank THK 1.2 TO 1.6 AND ONWORDS)

        PRODUCT RANGE  : A Wide Variety Of Coded And Non- Coded Equipment Manufacture At Larsen &Toubro Ltd. For Clients In India And Abroad. This Includes :

* Evaporates And Dryers, Vibro Fluidisers, Air Dispersers, Cyclones, Separators….. Silos And Tanks, Heat Exchangers, Pressure Vessels, Columns, Cryogenic Vessels, Custom-Built Fabricated Equipment, Aluminums Job Experience:
We Have Made A
1. Nitric Acid Storage Tanks Of Aluminums (Mat- Sb 1060 / Sb 1100 ) For Gnfc -Fertilizer Plant ,Bharuch-India
2. Oxy Generator Columns Of Aluminums (Mat- Sb 5083 ) For British Oxygen Company (Boc ) U.K .
COMPANY : Larsen & Toubro Ltd, Located At Baroda, Is A, India's Leading Engeering Organisation .Address Is: Larsen & Toubro Limited , plot no. 101 ,G.I.D.C. Ranoli, Baroda-391350 ,Gujarat ,India
I assure you that I shall justify my selection if given a chance to work with your esteemed organization.
Thank you .
Your's faithfully,
Darpan Patel

7/29/02

 

MECHANICAL ENGINEER, PLASMA. A Principal-level Mechanical Engineer with a specialty in the plasma cutting, welding or spraying industry who will develop designs and processes for advanced plasma cutting systems. Must have a background in compressible fluid dynamics, plasma physics, heat and mass transport and material science, DOX and laboratory instrumentation, knowledge of CFD, FEA, and statistical methods.
Thank you.

Dave Palmer
Recruiter
Palmer & Associates
Burlington, VT 05401
(802) 863-4478
david@palmerjobs.com


6/30/02

Title: Sr. Welding Engineer
Description: Job Requisition #8980
Sr. Welding Engineer
CAN Module Center
Pratt & Whitney Aircraft Engines

Responsibilities include development of welding processing on aerospace parts. Includes Tig, EB, Laser, etc. Has to have the ability to develop weld schedules for very complex parts. Must be a highly energetic individual, have the ability to work with teams, and must be able to work well with limited supervision.
BS Welding Engineering or Welding Engineering Technology required 3-5 years experience
Please email resume to bachroj@pweh.com with 'Welding Engineer #8980' in the subject line.

Jonna (Bachrow) Gerken
Human Resources Representative
CAN Module Center860-565-0638 ph
860-755-6073 fax
860-708-1885 pager
bachroj@pweh.com

6/30/02

POST APPLIED FOR WELDER
RESUME
NAME :  JAMES IJU JAMES.
FATHER’S NAME :  James.
DATE OF BIRTH:  3rd February 1973.
PLACE OF BIRTH :  Kollam, Kerala.
MARITAL STATUS:  Married.
PASSPORT DETAILS
PASSPORT No. :  Q 602185.
DATE OF ISSUE :  2nd November 1993.
PLACE OF ISSUE :  Trivandrum.
DATE OF EXPIRY:  1st November 2003.
PERMENENT ADDRESS:  Johmy Land, Koivila Post, Kollam, Kerala - 691 590.India.
PRESENT ADDRESS:  Old No. 6, New No. 13, Balaraman Street,Ganapathypuram, East Tambaram, Chennai - 600 059, Tamil Nadu, India. Ijujames@hotmail.com.
EDUCATIONAL QUALIFICATION:  Plus Two.
TECHNICAL QUALIFICATION :  Six months training for Welding Technology in Madras Institute of Technology Campus.
           One month practical training in Shielded Metal Arc Welding in Ador Institute of Welding Technology.(Advani - OERLIKON Ltd.,).
           One month practical training for Gas Shielded Metal Arc Welding and Gas Shielded Tungsten Arc Welding in Ador Institute of Welding Technology (Advani - OERLIKON Ltd.,).
WORK EXPERIENCE IN INDIA:  Seven years experience in India as a WELDER (S.M.A.W. 6G. G.M.A.W. and G.T.A.W.)
WORK EXPERIENCE IN ABROAD :  Two years experience in GULF PIPING COMPANY, ABUDHABI as a WELDER (S.M.A.W. 6G).
I am having a additional Good knowledge in F.C.A.W. and G.T.A.W.
 

1/20/2002


 

Metallurgical Welding Engineer


     Target Rock Corporation, a Division of Curtiss-Wright Flow Control Corporation, is currently seeking a Welding Engineer for our manufacturing facility in E. Farmingdale, NY. Successful candidate should be experienced with generating and qualifying procedures for manual and automated processes (GTAW, PTAW, Oxyacetylene). Hardsurfacing knowledge a plus. Must be able to interact and provide technical support to Engineering and Production personnel. Project Management experience a plus.
      Requires B.S. in Metallurgical Engineering and/or Welding Engineering. Knowledge of NAVSEA 250-1500-1 and ASME Code Section III and IX a plus.
     This is a full-time direct position. Salary is dependent on experience.

US Citizenship is REQUIRED.
Please forward resume to:
Sandi Visco
svisco@trc.curtisswright.com

(714) 491-3940 (voice)
(714) 491-3944 (fax)

9/6/2001



JESUS VALLADARES
1769 CHALADAY LANE
EAST MEADOW, NEW YORK, 11554
516 485 4581

OBJECTIVE
: A WELDING POSITION THAT WILL ENABLE ME TO UTILIZE MY SKILLS TO IT'S FULLEST POTENTIAL.
QUALIFICATIONS: ELECTRIC ARC, MIG, TIG, OXY ACETYLENE CUTTING/WELDING PLASMA ARC, ALUMINUM, STAINLESS STEEL, IRON, ANODIZED ALUMINUM CAST IRON, BRONZE, GALVANIZED.
EDUCATION 1991 GENERAL EQUIVALENCY DIPLOMA 1989 1G&2G CERTIFICATION , MIAMI LAKES TECHNICAL ED. CENTER FL.
EMPLOYMENT
 1992- HEAD WELDER, S.L. DOERY & SON LAWRENCE N.Y. BUILD COMMERCIAL AND RESIDENTIAL FRAMES SUPERVISE AWNING INSTALLATION OPERATE FLAT BED
1991 WELDER ,CUSTOM TANK SERVICE HIALEAH, FL TIG WELDED ALUMINUM/STAINLESS STEEL GAS/DIESEL/TANK ASSISTED OWNER IN PROVIDING RATES FOR CUSTOMERS INSTALLED GAUGES ON TANKS, REPAIRED USED TANKS INSTALLED AND WELDED BAFFLES
1990-1991 WELDER, PIPE TECH CORPORATION MIAMI RIVER FL BUILT, WELDED, INSTALLED ANODIZED FULL TOWERS FOR YACHTS BUILT HALF TOWERS, BOW/PULPIT RAILS, LADDERS/RADAR PLATES CALCULATED MEASUREMENTS FOR JOBS AND SKETCHED DRAFT OPERATED HYDRAULIC AND MANUAL PIPE BENDER
1988-1989 WELDER, FLORIDA MARINE TANKS MIAMI FL TANK WELDING BASED ON PIECE WORK FABRICATED AND WELDED DOOR FRAMES, WINDSHIELDS BUILT SIDE VENTS FOR BOATS ASSISTED WITH PROTOTYPE PROJECTS, SHIPPING AND RECEIVING OPERATED DRILL/SHEER PRESS, TABLE SAW, DIE BENDER
1989 WELDING SUPERVISOR, MAKO MARINE FL SUPERVISION OF TANK WELDING, PRODUCTION AND FABRICATION
1989 WELDER, HOBART WOLLARD AIRPORT EQUIPMENT CO HIALEAH FL BUILT AND WELDED GROUND EQUIPMENT FOR AIRLINES

5/26/2000


WELDERS
Steel, Aluminum (MIG & TIG)
Experienced Only
PT/FT, Days and Nights
Setauket Manufacturer
Call 631-751-7985

1/5/2000


MY NAME IS JOHN BAUER
EAST MORICHES,NY
E-MAIL CLASS1WELD@AOL.COM
I HAVE 13 YEARS WELDING EXPERIENCE.I HOLD A NYC CLASS 1 LICENSE,A AWS D1.1 CERT. AND NYS DOT CERT I'VE WELDED IN A SHIPYARD AND AM CURRENTLY WELDING FOR A CONSTRUCTION CO THAT BUILDS BRIDGES,PILEDRIVES,DOCKBUILDS,AND ALSO WORKED IN A STRUCTUAL STEEL SHOP FABRICATING AND ERECTING.I CAN TAKE OFF BLUEPRINTS FABRICATE USE A TORCH AND MIG WELD.I HAVE A CDL CLASS 1 DRIVING LICENSE AND HAVE HEAVY EQUIPMENT EXPERIENCE.I ALSO HAVE EXPERIENCE IN AND AROUND CRANES.FOR MORE INFO PLEASE E-MAIL ME AT THE ABOVE ADDRESS OR YOU CAN CALL ME AT (516)874-0625 THANKYOU

6/7/1999


Kenneth Messemer
813 Sixth Street
West Babylon, NY 11704
(516)884-3824
OCCUPATION: WELDER, 20 years experience
WORK HISTORY
Dyna- Empire, Inc. 8/97 to Present
Stewart Ave., Garden City, NY
Welder, full time. Welding of military grade thermo couples to precise tolerances. Expensive materials involved, such as platinum. Other job aspects are similar to previous aircraft experience.
Kenneth J. Herman, Inc. 3/97 to 8/97
45 Dixon Ave., Copiague, NY
Welder, full time for a moderate sized construction company. Various types of welding and fabrication, job lay out.
Grumman Corporation 3/95 to 5/96
Bethpage, NY
Welder, Heli-ARC – lon Collider for Grumman’s RHIC (Relativistic Heavy lon Collider) Program. Job duties included performing high- pressure vacuum vessel weldments utilizing automated equipment. Welding was done to code specifications and stringent company standards. Input of welding parameters into computer review welding operation via video monitoring system. This job required the ability to interpret and work from blueprints. This was a fifteen-month assignment.
BH Aircraft 2l94 to 3/95
441 Eastern Parkway, Farmingdale, NY
Work included mainly welding of aircraft parts. Various types of welding and materials used. Similar to work experience listed below for Grumman.
Grumman Corporation 3/80 to 9/93
Bethpage, NY
My responsibilities included those of acting lead person on my shift. Work experience includes one year in the assembly of jigs and fixtures, and 12 years in the assembly of tig welded stainless steel, inconel, titanium, aluminum and other aircraft materials. Most welding required to be of X-ray quality. My job required knowledge of precision assembly procedures. All work done from blueprints and all welding certified by the U.S. Navy.
Plascal Corp., Eastern Pkwy, Farmingdale 6/76 to 3/80
Fabrication of steel, stainless steel and a1uminum fixtures used in manufacture of vinyl.
EDUCATION
Graduate of Bay Shore High School, 1976, Bay Shore, NY Completed courses in welding and metal fabrication through BOCES
AFFILIATIONS
American Welding Society

Dear Sirs,
I'am currently seeking employment in the welding trade. I have NYC license class I. I'am very well qualified in stick, MIG, TIG, Torch, and Thermal Spraying processes. I'am skilled at welding steel, stainless steel, aluminum, magnesium, and copper alloys. Please send offers to

Darrel Trinko
124 Columbia Hgts
Brooklyn, New York 11201
718-625-3600
e-mail dglennl@snet.net
 

Chuck Gibson                                                                                                                        5/25/98
6611 E. 55th Street
Tulsa, OK 74145
Provide welding and welding related information in written and oral form to management, manufacturing and engineering departments. Provide technical support relating to welding, heat treatment and equipment needs.
Assure the continous application A. W. S. and A. S. M. E. code welding procedure specifications for the plant;
Support research and development of new and/or improved welding metals, welding processes, and welding equipment in order to provide filler metals, processes and welding equipment that will consistently provide manufacturing the best cost effective method of building products;
Interface with quality control and shop supervisors to perform welder performance qualification testing in accordance with A. W. S. and A. S. M. E. codes;
Interface with the engineering department with respect to weld joint design, welding methods to be used, advice on materials to be welded, and assignment of welding processes in the form of welding notes on fabrication drawings;
Assist in the disposition of “Non-conforming Materials Reports” regarding repair of in-process welding and material defect problems. Assist in solving plant problems related to welding and repair of broken pieces of manufacturing equipment;
Training and instruction on proper operation of welding/welding related equipment;
Development of welding, tooling and miscellaneous fixtures to promote economical manufacturing methods.
Must have :
One year experience in welding techniques, welding related equipment and shop drawing interpretation;
A minimum six months working with A. W. S. and A. S. M. E. codes and standards;
Must have a B. S. degree in Welding Engineering or Metallurgical Engineering.
Phone (918)627-4924    Fax (918)627-6851    email cogibson@webzone.net
Commercial Job sites for welding and manufacturing professionals
http://www.weldingjobs.com      http://www.materialsjobs.com    

07/29/02