35 Machinery D14.1/D14.1M:2005, Specification for Welding of Industrial and Mill Cranes and Other Material Handling Equipment Specifies requirements for welding of all principal structural weldments and all primary welds used to manufacture cranes for industrial, mill, powerhouse, and nuclear facilities. Applies to other overhead material-handling machinery and equipment that support and transport loads within the design rating, vertically or horizontally, during normal operations. When agreed upon between owner and manufacturer, it may apply to loading caused by abnormal operations or environmental events, such as seismic loading. All provisions apply to strengthening and repairing of existing overhead cranes and material handling equipment. Contains figures and tables with prequalified joint details, allowable stress ranges, stress categories, and nondestructive examination techniques. Does not apply to construction or crawler cranes or welding of rails. 150 pages, 60 figures, 21 tables (2005). Order Code: D14.1 $104/$78 D14.3/D14.3M:2010, Specification for Welding Earthmoving, Construction, and Agricultural Equipment For self-propelled, on- and off-highway machinery and agricultural equipment. Specifies requirements for structural welds used in the manufacture and repair of crawlers, tractors, graders, loaders, off-highway trucks, power shovels, backhoes, mobile cranes, draglines, and other heavy earthmoving, construction, and agricultural equipment. Provides exhaustive illustrations of prequalified complete and partial penetration welded joints (butt, corner, T-, or combination) for shielded metal arc welding, submerged arc welding, gas metal arc welding, and flux cored arc welding. Includes variables for prequalified fillet welds. Annexes include “Recommended Practices for Treatment of Shielded Metal Arc and Flux Cored Arc Electrodes.” Tables include “Weldability Classification—Typical Steel Products” and “Minimum Preheat and Interpass Temperatures.” 94 pages, 22 figures, 13 tables (2010). Order Code: D14.3 $80/$60 D14.4/D14.4M:2012, Specification for the Design of Welded Joints in Machinery and Equipment Specifies common acceptance criteria for carbon and low-alloy steel welded joints in machines and equipment subject to static and dynamic loading. Covers classification of welded joints, weld joint design, workmanship, quality control requirements and procedures, welding operator and procedure qualification, weld joint inspection (visual, radiographic, ultrasonic, magnetic particle, liquid penetrant), repair, and post weld treatments. Describes the effect of weld joint geometry, welding practices, and quality control on allowable stress levels, and provides practices for qualification and examination of welded joints in machinery and equipment fabrication. Contains figures and tables with prequalified joint details, nondestructive examination techniques, and weld-inspection criteria. 122 pages, 38 figures, 16 tables (2012). Order Code: D14.4 $92/$69 D14.5/D14.5M:2009, Specification for Welding of Presses and Press Components Presents the current minimum standards and guidelines for the welded fabrication and repair of presses and press components. Addresses classification, weld joint design, stresses, tolerances, welder qualification, and a welding quality program. 158 pages, 69 figures, 24 tables, 3 forms (2009). Order Code: D14.5 $104/$78 D14.6/D14.6M:2012, Specification for Welding of Rotating Elements of Equipment Specifies the requirements for weld joint detail and fabrication by welding of rotating elements for new equipment and modification or repair of existing equipment. Equipment types include, but not limited to: crushers, fans, impellers, centrifugal impellers, kilns,pulpers, gears, sheaves, drive trains, crankshafts, flywheels, power transmission shafts, air moving devices, blowers, and rotating elements of hydroelectric generation equipment. The intent of this specification is not to include steam or combustion turbine rotors, blading, or camshafts. This specification includes requirements for welding procedure and welder performance qualification and inspection and quality control and refers to AWS B2.1/B2.1M for base material specifications and groupings (BMG), tables for welding consumable F and A numbers, welding positions, test fixtures, macroetch procedures, and sample forms.. 86 pages, 10 tables, 19 figures (2012). Order Code: D14.6 $76/$57 D14.7/D14.7M:2005, Recommended Practices for Surfacing and Reconditioning of Industrial Mill Rolls Provides guidance on surfacing, repair, and reconditioning of industrial mill rolls in the heavy metals, paper, plastic, and lumber industries. Emphasizes the use of submerged arc welding, but also addresses gas metal arc welding, and flux cored arc welding, with suitable modifications. Applicable to electroslag cladding. Covers welding, postweld heat treating, finish machining, inspection, and record keeping. Provides detailed guidelines, tables, figures, and forms for use in establishing documented, qualified Welding Procedure Specifications. 66 pages, 20 figures, 13 tables (2005). Order Code: D14.7 $68/$51 D14.8M:2009(ISO/TR 17844:2004 IDT), Standard Methods for the Avoidance of Cold Cracks See page 21. NEW PUBLICATION: D14.9/D14.9M:2013, Specification for Welding of Hydraulic Cylinders Provides standards for the design and manufacture of pressure containing welded joints and structural welded joints used in the manufacture of hydraulic cylinders. Manufacturer’s responsibilities are presented as they relate to the welding practices that have been proven successful within the industry in the production of hydraulic cylinders. Included are sections defining welding procedure qualification, welding performance qualification, workmanship and quality requirements, as well as inspection requirements and repair requirements. 49 pages, 17 figures, 6 tables (2013) Order Code: D14.9 $68/$51 HEAVY MACHINERY BUNDLES Bundle E:2013 • D14.3/D14.3M:2010, Specification for Welding Earthmoving, Construction, and Agricultural Equipment • B2.1:/B2.1M:2009-ADD1, Specification for Welding Procedure and Performance Qualification Individual catalog prices would be $320/$240—SAVE $48/$36 Order Code: BUNDLE E:2013 $272/$204 Bundle F:2013 • D14.6/D14.6M:2012, Specification for Welding of Rotating Elements of Equipment • B2.1:/B2.1M:2009-ADD1, Specification for Welding Procedure and Performance Qualification Individual catalog prices would be $316/$237—SAVE $47/$35 Order Code: BUNDLE F:2013 $269/$202
AWS Publications Catalog | Summer 2013
To see the actual publication please follow the link above