Food Processing Systems D18.1/D18.1M:2009, Specification for Welding of Austenitic Stainless Steel Tube and Pipe Systems in Sanitary (Hygienic) Applications Specifies requirements for gas tungsten arc welding of austenitic stainless steel tube and pipe at least 1/4 inch (6 mm) diameter in the fabrication of sanitary processing systems for handling products for human and animal consumption. May also be applied to maintenance of food processing equipment. Addresses procedure and performance qualification, fabrication, visual examination requirements, and documentation. 34 pages, 2 figures (2009). Order Code: D18.1 $56/$42 D18.2:2009, Guide to Weld Discoloration Levels on Inside of Austenitic Stainless Steel Tube Laminated sheet with color photograph shows degrees of coloration inside an austenitic stainless steel tube with increasing amounts of oxygen in the backing shielding gas. Suitable as a specifying tool and visual examination guide. (2009). 81⁄2” X 11” Order Code: D18.2 $40/$30 13” X 19” Order Code: D18.2XL $52/$39 D18.3/D18.3M:2005, Specification for Welding of Tanks, Vessels, & Other Equipment in Sanitary (Hygienic) Applications Covers issues not addressed by D18.1, including welding of carbon steels, stainless steels, and nickel alloys for construction of new tanks and other equipment. Includes welding of pipe to sanitary equipment. 38 pages, 3 nonmandatory annexes, 2 figures, 3 tables (2005). Order Code: D18.3 $56/$42 Fully searchable Welding Journals from 1919 to 2012 are now available in their entirety on DVDs See page 3 Everyday Pocket Guides The Everyday Pocket Handbook for Arc Welding Steel Useful charts and drawings relevant to arc welding steel. Includes classification, size, amperes, and deposition rates for selected shielded metal arc welding, gas metal arc welding, and flux cored arc welding electrodes. Also covers weld positions, pipe size and wall thicknesses, basic welding symbols and locations, and guide to electrode conditioning and storage. 34 pages, spiral-bound. 31/2" x 6" (1994). Order Code: PHB-1 $20/$15 The Everyday Pocket Handbook for Visual Inspection and Weld Discontinuities—Causes and Remedies Covers cracks, inclusions, incomplete fusion, incomplete joint penetration, overlap, porosity, undercut, and weld profiles. Compiled from AWS sources by Ted Weber, principal consultant for Weber and Associates. 34 pages, spiralbound. 31/2" x 6" (2000). Order Code: PHB-2 $20/$15 The Everyday Pocket Handbook on Welded Joint Details for Structural Applications Twenty diagrams of structural joints with prequalified details from D1.1 in a pocket handbook format. 32 pages, spiralbound. 31/2" x 6" (Revised 2004). Order Code: PHB-3 $20/$15 The Everyday Pocket Handbook for Gas Metal Arc Welding (GMAW) and Flux Cored Arc Welding (FCAW) Includes shielding gas information for gas metal arc welding using spray arc transfer, short-circuiting arc transfer, globular to spray transition currents, arc voltages, wire-feed speed, melting rates, and typical welding conditions for carbon and low-alloy steels, stainless steels, and aluminum. Includes specification and classification system for flux cored arc welding electrodes, and same topics as gas metal arc welding portion for CO2 and selfshielding. Covers troubleshooting advice for mechanical and electrical gas metal arc welding and flux cored arc welding. 50 pages, spiral-bound. 31/2" x 6" (2000). Order Code: PHB-4 $20/$15 The Everyday Pocket Handbook on Metric Practices for the Welding Industry Includes table conversions for common welding terms, length conversions, electrode sizes, fillet weld sizes, welding travel and wire feed speeds, deposition rates, and gas flow rates. 24 pages, spiral-bound. 31/2" x 6" (2000). Order Code: PHB-5 $20/$15 The Everyday Pocket Handbook for Visual Inspection of AWS D1.1 Structural Welding Code’s Fabrication and Welding Requirements Compilation of excerpts from D1.1/D1.1M:2004. Includes transitions between unequal thickness, access hold requirements, pre-weld joint detail, base material surface and weld profile requirements, and five pages of visual acceptance criteria. Useful when actual D1.1 code is too cumbersome for tight, on-the-job areas. 38 pages, spiral-bound. 31/2" x 6" (Revised 2004). Order Code: PHB-6 $20/$15 The Everyday Pocket Handbook for Shielded Metal Arc Welding (SMAW) Emphasizes shielded metal arc welding electrode care, handling, and use. Includes convenient classification suffix charts, suggested amperage ranges, stub loss, electrode orientation, and suggested joint designs. 34 pages, spiralbound. 31/2" x 6" (1998). Order Code: PHB-7 $20/$15 The Everyday Pocket Handbook for Gas Metal Arc Welding (GMAW) of Aluminum Covers preparation of aluminum for welding, tips and troubleshooting, typical procedures for groove and fillet welds in aluminum alloys with argon shielding, aluminum filler metal properties (as-welded condition), and guide to selection of filler metal for general-purpose welding. 32 pages, spiral-bound. 31/2" x 6" (1998). Order Code: PHB-8 $20/$15 Resistance Welding Pocket Handbook See page 36. Lesser price shown is for AWS members. Always get the best price from the source: 888-WELDING 29
AWS Publications Catalog | Summer 2013
To see the actual publication please follow the link above