Page 27

AWS Publications Catalog | Summer 2013

BASE METAL THICKNESS PROCESS FILLER METAL CONDITION ORDER NO. Carbon Steel 1/8" – 1-1/2" ER70S-3 & E70T-1M, E71T-1M or -12M As-welded or PWHT B2.1-1-232:2006 Carbon Steel 1/8" – 1-1/2" ER70S-3 As-welded or PWHT B2.1-1-233:2006 Carbon Steel 1/8" – 1-1/2" FCAW-G, Ar-CO2 shielded E70T-1M, E71T-1M, or E71T-12M As-welded or PWHT B2.1-1-234:2006 Carbon Steel 1/8" – 1-1/2" GMAW spray transfer*** ER70S-3 As-welded or PWHT B2.1-1-235:2006 Carbon Steel 1/8" – 1-1/2" GTAW ER70S-2 As-welded or PWHT B2.1-1-207:1996(R2007) Carbon Steel 1/8" – 1-1/2" ER70S-2 & E7018 As-welded or PWHT B2.1-1-209:1996(R2007) Carbon Steel 1/8" – 1-1/2" INMs-1 & ER70S-2 As-welded or PWHT B2.1-1-210:2001(R2012) Carbon Steel 1/8" – 1-1/2" INMs-1, E70S-2 & E7018 As-welded or PWHT B2.1-1-211:2001(R2012) Carbon Steel 1/8" – 3/4" SMAW E6010 & E7018 As-welded B2.1-1-201:1996(R2007) Carbon Steel 1/8" – 3/4" SMAW E6010* & E7018 As-welded B2.1-1-202:1996(R2007) Carbon Steel 1/8" – 3/4" SMAW E6010 As-welded B2.1-1-203:1996(R2007) Carbon Steel 1/8" – 3/4" SMAW E6010* As-welded B2.1-1-204:1996(R2007) Carbon Steel 1/8" – 1-1/2" SMAW E6010 & E7018 As-welded or PWHT B2.1-1-205:1996(R2007) Carbon Steel 1/8" – 1-1/2" SMAW E6010* & E7018 As-welded or PWHT B2.1-1-206:1996(R2007) Carbon Steel 1/8" – 1-1/2" SMAW E7018 As-welded or PWHT B2.1-1-208:1996(R2007) Carbon to Stainless 1/16" – 1-1/2" GTAW ER309(L) As-welded B2.1-1/8-227:2002 Carbon to Stainless 1/8" – 1-1/2" ER309(L) & E309(L)-15,-16 or -17 As-welded B2.1-1/8-229:2002 Carbon to Stainless 1/16" – 1-1/2" IN309 and ER309(L) As-welded B2.1-1/8-230:2002 Carbon to Stainless 1/8" – 1-1/2" As-welded B2.1-1/8-231:2002 Carbon to Stainless 1/8" – 1-1/2" SMAW E309(L)-15,-16 or -17 As-welded B2.1-1/8-228:2002 Stainless Steel 1/16" – 1-1/2" GTAW ER3XX As-welded B2.1-8-212:2001(R2012) Stainless Steel 1/8" – 1-1/2" ER3XX & E3XX-XX As-welded B2.1-8-214:2001(R2012) Stainless Steel 1/8" – 1-1/2" IN3XX & ER3XX As-welded B2.1-8-215:2001(R2012) Stainless Steel 1/8" – 1-1/2" IN3XX, ER3XX & E3XX-XX As-welded B2.1-8-216:2001(R2012) Stainless Steel 1/8" – 1-1/2" SMAW E3XX-XX As-welded B2.1-8-213:1997(R2012) Cr-Mo (M-4/P-4) 1/8" – 3/4" GTAW ER80S-B2 B2.1-4-217:1999(R2009) Cr-Mo (M-4/P-4) 1/8" – 1-1/2" ER80S-B2 & E8018-B2 B2.1-4-219:1999(R2009) Cr-Mo (M-4/P-4) 1/8" – 3/4" IN515 & ER80S-B2 B2.1-4-220:1999(R2009) Cr-Mo (M-4/P-4) 1/8" – 1-1/2" IN515, ER80S-B2, & E8018-B2 B2.1-4-221:1999(R2009) Cr-Mo (M-4/P-4) 1/8" – 1-1/2" SMAW E8018-B2 B2.1-4-218:1999(R2009) Cr-Mo (M-5A/P-5A) 1/8" – 3/4" GTAW ER90S-B3 B2.1-5A-222:1999(R2009) Cr-Mo (M-5A/P-5A) 1/8" – 1-1/2" ER90S-B3 & E9018-B3 B2.1-5A-224:1999 Cr-Mo (M-5A/P-5A) 1/8" – 3/4" IN521 & ER90S-B3 B2.1-5A-225:1999(R2009) Cr-Mo (M-5A/P-5A) 1/8" – 1-1/2" IN521, ER90S-B3, & E9018-B3 B2.1-5A-226:1999 Cr-Mo (M-5A/P-5A) 1/8" – 1-1/2" SMAW E9018-B3 B2.1-5A-223:1999(R2009) 25 Let AWS Standard Welding Procedure Specifications (SWPSs) do the work for you. PRIMARILY PIPE CHROME-MOLY STEEL STAINLESS M-1 TO M-8 CARBON STEEL PRIMARILY PIPE ALL STANDARDS BELOW ARE ADOPTED BY NATIONAL BOARD INSPECTION CODE, except B2.1-1-202 GMAW-S followed by FCAW-G** GMAW-S followed by GMAW spray transfer*** GTAW followed by SMAW GTAW, consumable inserts As-welded (≤1/2") or PWHT (all thicknesses) As-welded (≤1/2") or PWHT (all thicknesses) As-welded (≤1/2") or PWHT (all thicknesses) As-welded (≤1/2") or PWHT (all thicknesses) As-welded (≤1/2") or PWHT (all thicknesses) As-welded (≤1/2") or PWHT (all thickness- As-welded (≤1/2") or PWHT (all thickness- As-welded (≤1/2") or PWHT (all thicknesses) As-welded (≤1/2") or PWHT (all thicknesses) As-welded (≤1/2") or PWHT (all thicknesses) IN309, ER309 & E309-15,-16 or -17, or ER309(L) &E309(L)-15,-16 or -17 GTAW, consumable inserts/SMAW GTAW followed by SMAW GTAW, consumable inserts GTAW, consumable inserts/SMAW GTAW followed by SMAW GTAW, consumable inserts GTAW, consumable inserts/SMAW GTAW followed by SMAW GTAW, consumable inserts GTAW, consumable inserts/SMAW GTAW followed by SMAW GTAW, consumable inserts GTAW, consumable inserts/SMAW **FCAW limited to uphill progression only when welding in the vertical position. ***GMAW spray transfer limited to flat position only. Most AWS publications are available for download, and can be previewed at pubs.aws.org


AWS Publications Catalog | Summer 2013
To see the actual publication please follow the link above