Page 31

Publications Catalog - Spring 2013

Food Processing Systems D18.1/D18.1M:2009, Specification for D18.3/D18.3M:2005, Specification for Welding of Austenitic Stainless Steel Tube Welding of Tanks,Vessels, & Other Equipment and Pipe Systems in Sanitary (Hygienic) in Sanitary (Hygienic) Applications Applications Covers issues not addressed by D18.1, including welding of car- Specifies requirements for gas tungsten arc welding of bon steels, stainless steels, and nickel alloys for construction of austenitic stainless steel tube and pipe at least 1/4 inch (6 new tanks and other equipment. Includes welding of pipe to mm) diameter in the fabrication of sanitary processing sanitary equipment. 38 pages, 3 nonmandatory annexes, 2 systems for handling products for human and animal figures, 3 tables (2005). consumption. May also be applied to maintenance of food Order Code: D18.3 $56/$42 processing equipment. Addresses procedure and performance qualification, fabrication, visual examination requirements, and documentation. 34 pages, 2 figures (2009). Fully searchable Order Code: D18.1 $56/$42 Welding Journals from 1919 to D18.2:2009, Guide to Weld Discoloration 2012 are now Levels on Inside of Austenitic Stainless available in their Steel Tube entirety on DVDs Laminated sheet with color photograph shows degrees of col- oration inside an austenitic stainless steel tube with increasing amounts of oxygen in the backing shielding gas. Suitable as a See page 2 specifying tool and visual examination guide. (2009). 81/2” X 11” Order Code: D18.2 $40/$30 13” X 19” Order Code: D18.2XL $52/$39 Everyday Pocket Guides The Everyday Pocket Handbook The Everyday Pocket Handbook on Metric for Arc Welding Steel Practices for the Welding Industry Useful charts and drawings relevant to arc welding steel. Includes table conversions for common welding terms, Includes classification, size, amperes, and deposition rates for length conversions, electrode sizes, fillet weld sizes, welding selected shielded metal arc welding, gas metal arc welding, and travel and wire feed speeds, deposition rates, and gas flow flux cored arc welding electrodes. Also covers weld positions, rates. 24 pages, spiral-bound. 31/2" x 6" (2000). pipe size and wall thicknesses, basic welding symbols and Order Code: PHB-5 $20/$15 locations, and guide to electrode conditioning and storage. 34 pages, spiral-bound. 31/2" x 6" (1994). The Everyday Pocket Handbook for Order Code: PHB-1 $20/$15 Visual Inspection of AWS D1.1 Structural Welding Code’s Fabrication and Welding The Everyday Pocket Handbook Requirements for Visual Inspection and Weld Compilation of excerpts from D1.1/D1.1M:2004. Includes Discontinuities—Causes and Remedies transitions between unequal thickness, access hold Covers cracks, inclusions, incomplete fusion, incomplete requirements, pre-weld joint detail, base material surface and joint penetration, overlap, porosity, undercut, and weld weld profile requirements, and five pages of visual acceptance profiles. Compiled from AWS sources by Ted Weber, principal criteria. Useful when actual D1.1 code is too cumbersome for consultant for Weber and Associates. 34 pages, spiralbound. tight, on-the-job areas. 38 pages, spiral-bound. 31/2" x 6" 31/2" x 6" (2000). (Revised 2004). Order Code: PHB-2 $20/$15 Order Code: PHB-6 $20/$15 The Everyday Pocket Handbook on Welded The Everyday Pocket Handbook for Joint Details for Structural Applications Shielded Metal Arc Welding (SMAW) Twenty diagrams of structural joints with prequalified details Emphasizes shielded metal arc welding electrode care, from D1.1 in a pocket handbook format. 32 pages, spiral- handling, and use. Includes convenient classification suffix bound. 31/2" x 6" (Revised 2004). charts, suggested amperage ranges, stub loss, electrode Order Code: PHB-3 $20/$15 orientation, and suggested joint designs. 34 pages, spiral- The Everyday Pocket Handbook for bound. 31/2" x 6" (1998). Gas Metal Arc Welding (GMAW) and Flux Order Code: PHB-7 $20/$15 Cored Arc Welding (FCAW) The Everyday Pocket Handbook for Gas Includes shielding gas information for gas metal arc welding Metal Arc Welding (GMAW) of Aluminum using spray arc transfer, short-circuiting arc transfer, globular to Covers preparation of aluminum for welding, tips and spray transition currents, arc voltages, wire-feed speed, melting troubleshooting, typical procedures for groove and fillet welds rates, and typical welding conditions for carbon and low-alloy in aluminum alloys with argon shielding, aluminum filler steels, stainless steels, and aluminum. Includes specification and metal properties (as-welded condition), and guide to classification system for flux cored arc welding electrodes, and selection of filler metal for general-purpose welding. 32 same topics as gas metal arc welding portion for CO2 and self- pages, spiral-bound. 31/2" x 6" (1998). shielding. Covers troubleshooting advice for mechanical and Order Code: PHB-8 $20/$15 electrical gas metal arc welding and flux cored arc welding. 50 pages, spiral-bound. 31/2" x 6" (2000). Resistance Welding Pocket Handbook Order Code: PHB-4 $20/$15 See page 36. Lesser price shown is for AWS members. Always get the best price from the source: 888-WELDING 29


Publications Catalog - Spring 2013
To see the actual publication please follow the link above