Development and qualification of welding procedures can be time-consuming and expensive. BASE METAL THICKNESS PROCESS FILLER METAL CONDITION ORDER NO. . SHEET METAL Carbon Steel 10 – 18 gauge GMAW-S ER70S-6 As-welded, with or w/o backing B2.1-1-004:2002 L E E T S Carbon Steel 10 – 18 gauge GTAW ER70S-2 or -3 As-welded, with or w/o backing B2.1-1-008:2002 N O B R A Carbon Steel 10 – 18 gauge SMAW E6010 or E6013 As-welded, with or w/o backing B2.1-1-012:2002 C Galvanized Steel 10 – 18 gauge GMAW-S ER70S-6 As-welded, with or w/o backing B2.1-1-003:2002 D E I Galvanized Steel 10 – 18 gauge GTAW ER70S-2 or -3 As-welded, with or w/o backing B2.1-1-007:2002 N A L L A Galvanized Steel 10 – 18 gauge SMAW E6010 or E6013 As-welded, with or w/o backing B2.1-1-011:2002 G T E M Carbon to Stainless 10 – 18 gauge GMAW-S ER309 As-welded, with or w/o backing B2.1-1/8-006:2002 T - E M Carbon to Stainless 10 – 18 gauge GTAW ER309 As-welded, with or w/o backing B2.1-1/8-010:2002 H O T S - Carbon to Stainless 10 – 18 gauge SMAW E309-15,-16 or -17 As-welded, with or w/o backing B2.1-1/8-014:2002 M Stainless Steel 10 – 18 gauge GMAW-S ER3XX As-welded, with or w/o backing B2.1-8-005:2002 S S E Stainless Steel 10 – 18 gauge GTAW ER3XX As-welded, with or w/o backing B2.1-8-009:2002 L I T S Stainless Steel 10 – 18 gauge SMAW E3XX-15,-16 or -17 As-welded, with or w/o backing B2.1-8-013:2002 Aluminum 10 – 18 gauge GTAW ER4043 or R4043 As-welded, with or w/o backing B2.1-22-015:2011 L A PLATE (ALL STANDARDS BELOW ARE ADOPTED BY NATIONAL BOARD INSPECTION CODE ) Carbon Steel 3/16" – 7/8" GTAW ER70S-2 or -3 As-welded, with or w/o backing B2.1-1-002:1990(R2006) Carbon Steel 1/8" – 1-1/2" GTAW followed ER70S-2 & E7018 As-welded or PWHT B2.1-1-021:1994 by SMAW Carbon Steel 3/16" – 3/4" SMAW E7016 & E7018 As-welded, with backing B2.1-1-001:1990(R2006) Carbon Steel 1/8" – 1-1/2" SMAW E7018 As-welded or PWHT B2.1-1-016:1994 Carbon Steel 1/8" – 1-1/2" SMAW E6010 As-welded or PWHT B2.1-1-017:1994 L E E T S Carbon Steel 1/8" – 1-1/2" SMAW E6010 & E7018 As-welded or PWHT B2.1-1-022:1994 N O B R A Carbon Steel 1/8" – 1-1/2" SMAW E6010* & E7018 As-welded or PWHT B2.1-1-026:1994 C T A L Carbon Steel 1/8" – 1-1/2" FCAW, E71T-8 As-welded B2.1-1-018:1994 P self-shielded Carbon Steel 1/8" – 1/2" FCAW, E71T-11 As-welded B2.1-1-027:2011 self-shielded Carbon Steel 1/8" – 1-1/2" FCAW-G, CO2 E70T-1 or E71T-1 As-welded B2.1-1-019:1994 gas-shielded Carbon Steel 1/8" – 1-1/2" FCAW-G, Ar-CO2 E70T-1 or E71T-1 As-welded or PWHT B2.1-1-020:1994 gas-shielded Stainless Steel 1/16" – 1-1/2" GTAW ER3XX As-welded B2.1-8-024:2001(R2012) S S Stainless Steel 1/8" – 1-1/2" GTAWSfMlAWed ER3XX & E3XX-XX As-welded B2.1-8-025:2001(R2012)woloyb E L I A T S Stainless Steel 1/8" – 1-1/2" SMAW E3XX-XX As-welded B2.1-8-023:1994 *Downhill progression on root pass. All other vertical position passes are uphill. Specifications with order numbers indicated in red are adopted by ASME with additional requirements. PRICES: The user-license one-time fee for each SWPS is $186 ($248 for nonmembers). AWS publishes Standard Welding Procedure Specifications (SWPSs), which are reviewed and validated by the Welding Procedures Committee of the Welding Research Council. They are balloted through the AWS standards- development program as American National Standards. Standard Welding Procedure Specifications may be used on work covered by the AWS D1.1, Structural Welding Code—Steel with the engineer’s approval. The National Board Inspection Code has adopted all pipe SWPSs except B2.1-1-202. SWPSs with red order numbers may be used on ASME Boiler and Pressure Vessel work with additional requirements spelled out in Section IX of ASME Boiler & Pressure Vessel Code. All licenses are good for unlimited intracompany applications. 24 Lesser price shown is for AWS members. Always get the best price from the source: 888-WELDING
Publications Catalog - Spring 2013
To see the actual publication please follow the link above